We want the fixed sensor (KMA221)by low pressure injection molding.
Injection molding temperature: 220℃-240s℃
Cycle time: 15-20sec
Is it feasible?
Dear Zhang,
Thank you for your interest in the KMA221, but unfortunately this is not feasible.
Best regards,
Tomas
Thank you for your reply.
why?High temperature?
Do you have any suggestions?
How about epoxy resin?